UNITED CHEMICAL · تكنولوجيا المنتج · 27 نوفمبر 2026
استخدم كربون you replace is not the carbon you lose
Fines carry gold out of the circuit, and they rarely appear on the purchase order.
Activated carbon is consumed two ways. It leaves as loaded carbon after elution, and it grinds into fines that report to tailings carrying adsorbed gold. The second loss is rarely budgeted. Ball-pan hardness and AARL attrition predict it; mesh size and platelet count predict how fast it happens in a given circuit. This guide uses كربون جوز الهند المنشط AuCarb™ Gold Recovery (صلابة ≥99%) as the worked example.
1. Three steps from solution to loaded carbon
Film diffusion — the [Au(CN)₂]⁻ complex crosses the solution boundary layer around each granule. Agitation controls this step.
Pore diffusion — the complex travels into internal pores. Granule size and pore structure control this step.
الامتزاز السطحي — the complex binds to active sites. Surface chemistry and total area control this step.
2. Why hardness is a recovery parameter
A granule that breaks in a stirred tank shortens diffusion paths but creates gold-bearing fines that escape the adsorption circuit. In an abrasive ore, moving from a marginal product to one at ball-pan hardness ≥99% with AARL attrition ≤1.5% cuts fines generation directly. The AC50 verified data set is: 6×12 mesh, ball-pan ≥99%, AARL attrition ≤1.5%, platelet ≤5.0%, K ≥26 kg/t, R ≥50%, CTC ≥50%, butane ≥19.5%, ash ≤3.0%, moisture ≤5.0%, bulk density 0.48–0.55 g/mL. Iodine value is deliberately omitted — published figures conflict, so CTC and butane activity are the auditable measures.
المثلث الذهبي - ثلاثة منتجات، مورد واحد
سيانيد الصوديوم AuCyan™ (≥98.3%) · الكربون المنشط من قشور جوز الهند AuCarb™ (صلابة ≥99%) · عامل استخلاص الذهب AuLeach™ (GDA) – غير ضار
3. Worked calculation: the cost of fines
A 2,000 t/day CIL plant carries 12 tonnes of carbon with a 30-day cycle. At 1.5% attrition per cycle it loses about 180 kg per cycle, or 2.2 tonnes a year. At 3.0% it loses roughly 4.3 tonnes — a difference of 2.1 tonnes of carbon. If those fines carry even 200 g/t of gold, the annual gold difference is about 420 g. At any reasonable gold price, the hardness premium paid for the better carbon is smaller than the gold saved.
1.5% attrition: ≈ 2.2 t/year make-up carbon
3.0% attrition: ≈ 4.3 t/year make-up carbon
4. K and R are not the same number
K value is the adsorption rate constant — how fast gold loads. R value is equilibrium capacity — how much it holds. A high K with modest R suits short contact time. A high R suits a circuit that runs carbon to heavy loading before elution. Buying on either alone is a common and expensive mistake. Run bottle-roll loading on your own ore, set the K/R target from your contact time, then buy the lowest grade that reaches it.
5. أربع درجات، أربع وظائف
| الصف | دائرة كهربائية | تحديد المواصفات |
|---|---|---|
| BC1100 | الترشيح بالكومة / الكربون في العمود | نشاط عالٍ للمحاليل منخفضة الجودة |
| AC50 | Standard CIP/CIL | 6×12 mesh, K ≥26, R ≥50%, CTC ≥50% |
| AC55 | CIP/CIL ذو التحميل الأعلى | K ≥ 28 كجم/طن، R ≥ 55% |
| AC60 | برنامج CIP/CIL الممتاز | K ≥ 30 كجم/طن، R ≥ 60%، 8×16 أو 6×12 |
6. التجديد ودورة الحياة
Loaded carbon is eluted and thermally regenerated before returning to the circuit. Every cycle imposes thermal and mechanical stress. Platelets and weak granules are preferentially lost in handling and regeneration. A carbon at ball-pan hardness ≥99% with platelet ≤5.0% typically sustains more cycles before make-up is required. Packing is أكياس بولي إيثيلين مغلفة شديدة التحمل بوزن 25 كجم, with a batch COA, TDS و ورقة بيانات سلامة المواد MSDSالحد الأدنى للطلب هو حاوية كاملة بطول 20 قدمًا ≈ 15 طنًا متريًا مع FOB / CIF شروط؛ United Chemical تخدم أكثر من 77 دولة.
5b. Screening and fines recovery
Attrition control does not end at the carbon specification. Screen condition determines whether a broken granule is removed cleanly or ground further and carried forward. A worn screen with oversized apertures passes loaded fines into the tailings stream; a blinded screen holds carbon in the tank too long and increases grinding. The practical routine is to log screen aperture, inspect panels on a fixed schedule and sample the carbon size distribution in the circuit monthly. If the proportion of sub-millimetre material is rising while make-up carbon is on budget, the problem is mechanical rather than metallurgical. Equally, gold-bearing fines caught on a screen are not lost; they should be routed to the elution circuit where the recovery economics justify it. This is why hardness and attrition numbers belong in an operating dashboard, not only in the purchase order.
7. التعليمات
س1 - ماذا يعني مصطلح "صلابة ≥99%" عملياً؟
Ball-pan hardness ≥99% means the granule resists mechanical breakdown to a defined standard, reducing fines.
Q2 — Which mesh size?
6×12 for agitated CIP/CIL, 8×16 where finer loading is needed, BC1100 for columns and heap.
س3 - هل تنشرون قيمة اليود؟
No — CTC and butane activity are the auditable pore measures because published iodine figures conflict.
س4 - ما الذي يتم شحنه مع كل دفعة؟
شهادة تحليل الدفعة، والبيانات الفنية، وبيانات سلامة المواد في أكياس بولي إيثيلين مغلفة شديدة التحمل سعة 25 كجم.
س5 - ما هو الحد الأدنى لكمية الطلب؟
1×20' FCL ≈ 15 طن متري، FOB أو CIF.
Q6 — Can I test before buying?
نعم - عينات مجانية من AuCarb™ و AuLeach™ لإجراء اختبارات معملية مستقلة.
Measure your attrition loss
Tell us your circuit type, screen aperture and ore abrasiveness. We propose a grade, a K/R target and a test protocol.
اتصل بنا · AC50 · AC55 · AC60 · نظرة عامة على المثلث الذهبي
واتساب +86 173 9270 5576 info@unitedchemicalcn.com
- محتوى عشوائي
- محتوى ساخن
- محتوى المراجعة الساخن
- مصنع الصين حمض الكبريتيك 98٪
- حمض الكبريتيك 98% درجة صناعية
- أنبوب صدمة بلاستيكي (VOD ≧ 1600 م/ثانية)
- كبريتات الحديدوز الصناعية 90%
- هل مواد التعويم لها تأثيرات بيئية؟
- 1سيانيد الصوديوم المخفض السعر (CAS: 143-33-9) للتعدين - جودة عالية وأسعار تنافسية
- 2سيانيد الصوديوم 98.3%، رقم CAS 143-33-9، عامل معالجة الذهب NaCN، ضروري للصناعات الكيميائية التعدينية
- 3اللوائح الصينية الجديدة بشأن صادرات سيانيد الصوديوم وإرشادات للمشترين الدوليين
- 4شهادة المستخدم النهائي لسيانيد الصوديوم (CAS: 143-33-9) (النسخة الصينية والإنجليزية)
- 5قانون إدارة السيانيد الدولي (سيانيد الصوديوم) - معايير قبول مناجم الذهب
- 6مصنع الصين حمض الكبريتيك 98٪
- 7حمض الأكساليك اللامائي 99.6% درجة صناعية
- 1سيانيد الصوديوم 98.3%، رقم CAS 143-33-9، عامل معالجة الذهب NaCN، ضروري للصناعات الكيميائية التعدينية
- 2نقاء عالي · أداء مستقر · استرداد أعلى - سيانيد الصوديوم لاستخلاص الذهب الحديث
- 3United Chemicalيُظهر فريق البحث في "" سلطته من خلال الرؤى القائمة على البيانات
- 4سيانيد الصوديوم عالي الأداء AuCyan™ | نقاء 98.3% لتعدين الذهب العالمي
- 5المفجر الإلكتروني الرقمي (وقت التأخير 0 ~ 16000 مللي ثانية)
- 6مفجر أنبوب الصدمة عالي القوة والدقة
- 7صناعة المفجر الكهربائي











استشارة الرسائل عبر الإنترنت
أضف تعليق: