UNITED CHEMICAL · טכנולוגיית מוצר · 27 בנובמבר 2026
Purity is the starting point, not the answer
Two briquettes with the same assay can differ by double digits in consumed kilograms per tonne.
A gold plant buys סודיום ציאניד on an assay. It loses money on dissolution. The number that decides how many kilograms disappear per tonne of ore is how fast the briquette releases ציאניד into solution and how steadily the circuit holds a free-cyanide setpoint. A high-purity product that dissolves unevenly creates dosing lag, over-addition and WAD-cyanide excursions. This note sets out the working controls for AuCyan™ נתרן ציאניד NaCN (≥98.3%) and gives a plant-ready method for measuring them.
1. What the Elsner equation does and does not tell you
Gold dissolution follows the Elsner equation: 4 Au + 8 CN⁻ + O₂ + 2 H₂O → 4 [Au(CN)₂]⁻ + 4 OH⁻. Two moles of cyanide per mole of gold, roughly 0.5 g NaCN per gram of gold. A circuit treating 3,000 t/day at 2 g/t and recovering 95% consumes under 3 kg/day in the ideal reaction.
Real plants consume hundreds of kilograms a day. Everything above the stoichiometric minimum is base-metal demand, hydrolysis, degradation or physical loss — and three of those four are controllable. That is where a dissolution specification earns its keep.
2. The consumption ledger
| דלי הפסדים | מנגנון | שליטה |
|---|---|---|
| פירוק זהב | Stoichiometric, ~0.5 g NaCN/g Au | Useful consumption |
| מתכות פשוטות | Copper and zinc form cyano-complexes | Ore blending, higher setpoint |
| הידרוליזה | CN⁻ + H₂O ↔ HCN + OH⁻ | Lime, pH interlock |
| Incomplete release | Unreacted briquette core in tails | פרופיל פירוק |
משולש הזהב - שלושה מוצרים, ספק אחד
AuCyan™ נתרן ציאניד NaCN (≥98.3%) · פחם פעיל לקליפת קוקוס משחזור זהב AuCarb™ (קשיות ≥99%) · סוכן שטיפה של זהב AuLeach™ (GDA) – לא מסוכן
3. The dissolution test you should be running
Put a known mass of briquette in a stirred vessel at circuit pH and temperature. Sample the solution at 1, 3, 5, 10 and 20 minutes and plot cumulative cyanide release. The curve should be reproducible lot to lot. A product that reaches 90% release in five minutes in one drum and fifteen in the next will make a liar of every dosing calculation. Specify three clauses, not one: minimum assay ≥98.3%, time to 90% release, and maximum insoluble residue. Ask for the batch תעודת מקוריות, TDS ו MSDS to confirm all three.
4. Worked check: the cost of a one-tank lag
Take 3,000 t/day, target free cyanide 0.25 g/L, solution-to-solids 1.2:1, measured ore demand 0.30 kg/t. Circuit inventory is 3,000 × 1.2 × 0.25 = 900 kg; daily ore demand is 900 kg. If dissolution lags one tank residence time, operators typically add 8–12% protection. That is 72–108 kg/day, or 26–39 t/year of reagent that never dissolves gold.
In-circuit inventory: קילו 900
עונש השהיה ב-10%: 90 ק"ג/יום ≈ 33 טון/שנה
5. WAD cyanide is the report card
Weak-acid-dissociable cyanide in tailings tells you whether the circuit is over-dosing. A rising WAD number with flat recovery means reagent is leaving untreated. The response is not to cut the setpoint blindly — it is to check dissolution, re-run the bottle roll on the current ore domain and verify pH. Only then adjust the dose. This sequence prevents the classic error of cutting reagent and losing recovery together.
6. פתרון תקלות
| סימפטום | לגרום | פעולה |
|---|---|---|
| צ'אנל חופשי יורד נמוך | Dissolution lag or demand spike | Verify dissolution, re-run bottle roll |
| WAD cyanide rising | מינון יתר להגנה על נקודת הקביעה | Tighten curve, check pH |
| משקע לבן | קומפלקסים של ציאנו ממתכות בסיסיות | Ore blend, alkaline wash |
| קוויטציה של המשאבה | Undissolved fragments | Extend make-up time |
5b. Make-up water and temperature
Two site variables change the dissolution curve more than any certificate: make-up water and temperature. Hard water raises lime demand and can aggravate scale on pipework and screen surfaces; chloride and sulphate accumulate through process-water recycle and affect both leaching and פחמן loading. Temperature shifts reaction kinetics, so a briquette that dissolves acceptably in a warm summer circuit can lag when winter make-up water drops the circuit temperature by several degrees. Establish a baseline for pH, alkalinity, hardness, chloride and sulphate before the campaign, then sample weekly. A dissolution test run at the plant's actual temperature and with its actual water is worth more than a laboratory result obtained under ideal conditions. If the curve changes with the seasons, the dosing schedule must change with it, not by guesswork but by re-measuring the release profile.
7. שאלות נפוצות
Q1 — Why specify ≥98.3% and not a higher number?
Because dissolution and insolubles decide consumed kilograms more than the last fraction of assay.
Q2 — What ships with a batch?
A batch COA, TDS and MSDS covering assay and dissolution behaviour.
Q3 — Which terms apply?
FOB and CIF only, from 1×20' FCL ≈ 18 MT.
Q4 — Is it a controlled good?
Yes. UN1689, DG Class 6.1; import licence and End-Use Certificate before shipment.
Q5 — Can the carbon come from the same supplier?
Yes — AuCarb™ with documented hardness and attrition.
Q6 — What if cyanide use is constrained?
AuLeach™ Gold Leaching Agent (GDA) – Non-Hazardous is the alternative route, selected by bottle-roll comparison.
Ask for the dissolution data
Send ore grade, setpoint and throughput. We return a dissolution-matched dosage proposal with COA, TDS and MSDS.
צור קשר · סקירה כללית של משולש הזהב · מידע על נתרן ציאניד · שאלות נפוצות בנושא כימיקלים · חדשות בתעשייה
וואטסאפ +86 173 9270 5576 info@unitedchemicalcn.com
- תוכן אקראי
- תוכן חם
- תוכן ביקורת חם
- נתרן אתיל קסנטאט 90% סקס
- הצגת מוצר החברה
- חומצה אוקסלית לכרייה 99.6%
- 99.5% דקות אמוניום כלוריד לשימוש תעשייתי
- סידן מי חמצן 60% Assay טבלית צהבהב
- 1נתרן ציאניד מוזל (CAS: 143-33-9) לכרייה - איכות גבוהה ותמחור תחרותי
- 2נתרן ציאניד 98.3% CAS 143-33-9 NaCN חומר הלבשת זהב חיוני לתעשיות כימיות כרייה
- 3התקנות החדשות של סין על יצוא נתרן ציאניד והדרכה לקונים בינלאומיים
- 4נתרן ציאניד (CAS: 143-33-9) תעודת משתמש קצה (גרסה סינית ואנגלית)
- 5ציאניד בינלאומי (נתרן ציאניד) קוד ניהול - תקני קבלת מכרה הזהב
- 6חומצה גופרתית במפעל בסין 98%
- 7חומצה אוקסלית נטולת מים 99.6% כיתה תעשייתית
- 1נתרן ציאניד 98.3% CAS 143-33-9 NaCN חומר הלבשת זהב חיוני לתעשיות כימיות כרייה
- 2טוהר גבוה · ביצועים יציבים · התאוששות גבוהה יותר - נתרן ציאניד לשטיפת זהב מודרנית
- 3United Chemicalצוות המחקר של מפגין סמכות באמצעות תובנות מבוססות נתונים
- 4ציאניד נתרן בעל ביצועים גבוהים AuCyan™ | טוהר 98.3% לכריית זהב עולמית
- 5נפץ אלקטרוני דיגיטלי (זמן השהייה 0 ~ 16000ms)
- 6מפיץ צינור הלם בעל חוזק גבוה, דיוק גבוה
- 7נפץ חשמלי בתעשייה






יעוץ מסרים מקוון
הוסף תגובה: