UNITED CHEMICAL · TECHNOLOGIE PRODUIT · 27 NOVEMBRE 2026
Le Carbon you replace is not the carbon you lose
Fines carry gold out of the circuit, and they rarely appear on the purchase order.
Activated carbon is consumed two ways. It leaves as loaded carbon after elution, and it grinds into fines that report to tailings carrying adsorbed gold. The second loss is rarely budgeted. Ball-pan hardness and AARL attrition predict it; mesh size and platelet count predict how fast it happens in a given circuit. This guide uses AuCarb™ Gold Recovery, charbon actif de coque de noix de coco (dureté ≥ 99 %) as the worked example.
1. Three steps from solution to loaded carbon
Film diffusion — the [Au(CN)₂]⁻ complex crosses the solution boundary layer around each granule. Agitation controls this step.
Pore diffusion — the complex travels into internal pores. Granule size and pore structure control this step.
Adsorption superficielle — the complex binds to active sites. Surface chemistry and total area control this step.
2. Why hardness is a recovery parameter
A granule that breaks in a stirred tank shortens diffusion paths but creates gold-bearing fines that escape the adsorption circuit. In an abrasive ore, moving from a marginal product to one at ball-pan hardness ≥99% with AARL attrition ≤1.5% cuts fines generation directly. The AC50 verified data set is: 6×12 mesh, ball-pan ≥99%, AARL attrition ≤1.5%, platelet ≤5.0%, K ≥26 kg/t, R ≥50%, CTC ≥50%, butane ≥19.5%, ash ≤3.0%, moisture ≤5.0%, bulk density 0.48–0.55 g/mL. Iodine value is deliberately omitted — published figures conflict, so CTC and butane activity are the auditable measures.
Le Triangle d'or — trois produits, un fournisseur
AuCyan™ Cyanure de sodium NaCN (≥98.3 %) · AuCarb™ Charbon actif de coque de noix de coco pour la récupération de l'or (≥99 % de dureté) · AuLeach™ Agent de lixiviation de l'or (GDA) – Non dangereux
3. Worked calculation: the cost of fines
A 2,000 t/day CIL plant carries 12 tonnes of carbon with a 30-day cycle. At 1.5% attrition per cycle it loses about 180 kg per cycle, or 2.2 tonnes a year. At 3.0% it loses roughly 4.3 tonnes — a difference of 2.1 tonnes of carbon. If those fines carry even 200 g/t of gold, the annual gold difference is about 420 g. At any reasonable gold price, the hardness premium paid for the better carbon is smaller than the gold saved.
1.5% attrition: ≈ 2.2 t/year make-up carbon
3.0% attrition: ≈ 4.3 t/year make-up carbon
4. K and R are not the same number
K value is the adsorption rate constant — how fast gold loads. R value is equilibrium capacity — how much it holds. A high K with modest R suits short contact time. A high R suits a circuit that runs carbon to heavy loading before elution. Buying on either alone is a common and expensive mistake. Run bottle-roll loading on your own ore, set the K/R target from your contact time, then buy the lowest grade that reaches it.
5. Quatre niveaux, quatre métiers
| Niveau | Circuit | Spécification de définition |
|---|---|---|
| BC1100 | lixiviation en tas / Carbone en colonne | Activité élevée pour les solutions de qualité inférieure |
| AC50 | Standard CIP/CIL | 6×12 mesh, K ≥26, R ≥50%, CTC ≥50% |
| AC55 | CIP/CIL à charge plus élevée | K ≥ 28 kg/t, R ≥ 55 % |
| AC60 | CIP/CIL Premium | K ≥ 30 kg/t, R ≥ 60 %, 8×16 ou 6×12 |
6. Régénération et cycle de vie
Loaded carbon is eluted and thermally regenerated before returning to the circuit. Every cycle imposes thermal and mechanical stress. Platelets and weak granules are preferentially lost in handling and regeneration. A carbon at ball-pan hardness ≥99% with platelet ≤5.0% typically sustains more cycles before make-up is required. Packing is Sacs en PE laminé haute résistance de 25 kg, with a batch COA, TDS et MSDSLa quantité minimale de commande est de 1 conteneur de 20 pieds (FCL) ≈ 15 tonnes métriques sous FOB / CAF termes; United Chemical dessert plus de 77 pays.
5b. Screening and fines recovery
Attrition control does not end at the carbon specification. Screen condition determines whether a broken granule is removed cleanly or ground further and carried forward. A worn screen with oversized apertures passes loaded fines into the tailings stream; a blinded screen holds carbon in the tank too long and increases grinding. The practical routine is to log screen aperture, inspect panels on a fixed schedule and sample the carbon size distribution in the circuit monthly. If the proportion of sub-millimetre material is rising while make-up carbon is on budget, the problem is mechanical rather than metallurgical. Equally, gold-bearing fines caught on a screen are not lost; they should be routed to the elution circuit where the recovery economics justify it. This is why hardness and attrition numbers belong in an operating dashboard, not only in the purchase order.
7. FAQ
Q1 — Que signifie en pratique une dureté ≥99 % ?
Ball-pan hardness ≥99% means the granule resists mechanical breakdown to a defined standard, reducing fines.
Q2 — Which mesh size?
6×12 for agitated CIP/CIL, 8×16 where finer loading is needed, BC1100 for columns and heap.
Q3 — Publiez-vous la valeur d'iode ?
No — CTC and butane activity are the auditable pore measures because published iodine figures conflict.
Q4 — Qu'est-ce qui est expédié avec chaque lot ?
Lot de certificats d'analyse (COA), fiches techniques (TDS) et fiches de données de sécurité (MSDS) dans des sacs en PE laminés haute résistance de 25 kg.
Q5 — Quel est le MOQ ?
1×20' FCL ≈ 15 MT, FOB ou CIF.
Q6 — Can I test before buying?
Oui — des échantillons gratuits d'AuCarb™ et d'AuLeach™ pour des tests en laboratoire indépendants.
Measure your attrition loss
Tell us your circuit type, screen aperture and ore abrasiveness. We propose a grade, a K/R target and a test protocol.
Contactez-Nous · AC50 · AC55 · AC60 · Aperçu du Triangle d'Or
WhatsApp +86 173 9270 5576 info@unitedchemicalcn.com
- Contenu aléatoire
- Contenu chaud
- Contenu de révision à chaud
- Acide sulfurique à 98 % fabriqué en Chine
- Acide sulfurique 98 % de qualité industrielle
- Tube à choc en plastique (VOD ≧ 1600 m/s)
- Sulfate ferreux de qualité industrielle 90 %
- Les réactifs de flottation ont-ils des impacts environnementaux ?
- 1Cyanure de sodium à prix réduit (CAS : 143-33-9) pour l'exploitation minière - Haute qualité et prix compétitifs
- 2Cyanure de sodium 98.3 % CAS 143-33-9 NaCN, agent de traitement de l'or, essentiel pour les industries chimiques minières.
- 3Nouvelle réglementation chinoise sur les exportations de cyanure de sodium et conseils aux acheteurs internationaux
- 4Cyanure de sodium (CAS : 143-33-9) Certificat d'utilisateur final (versions chinoise et anglaise)
- 5Code international de gestion du cyanure (cyanure de sodium) - Normes d'acceptation des mines d'or
- 6Acide sulfurique à 98 % fabriqué en Chine
- 7Acide oxalique anhydre 99.6 % de qualité industrielle
- 1Cyanure de sodium 98.3 % CAS 143-33-9 NaCN, agent de traitement de l'or, essentiel pour les industries chimiques minières.
- 2Haute pureté · Performances stables · Récupération supérieure — cyanure de sodium pour la lixiviation moderne de l'or
- 3United ChemicalL'équipe de recherche de démontre son autorité grâce à des informations basées sur les données
- 4AuCyan™ Cyanure de sodium haute performance | Pureté de 98.3 % pour l'exploitation minière de l'or à l'échelle mondiale
- 5Détonateur électronique numérique (temps de retard 0 à 16000 XNUMX ms)
- 6Détonateur à tube à choc de haute résistance et de haute précision
- 7Détonateur électrique industriel











Consultation des messages en ligne
Ajouter un commentaire: