UNITED CHEMICAL · TECNOLOGIA DI PRODOTTO · 27 NOVEMBRE 2026
Migliori Carbonio you replace is not the carbon you lose
Fines carry gold out of the circuit, and they rarely appear on the purchase order.
Activated carbon is consumed two ways. It leaves as loaded carbon after elution, and it grinds into fines that report to tailings carrying adsorbed gold. The second loss is rarely budgeted. Ball-pan hardness and AARL attrition predict it; mesh size and platelet count predict how fast it happens in a given circuit. This guide uses AuCarb™ Gold Recovery Carbone attivo da guscio di cocco (durezza ≥99%) as the worked example.
1. Three steps from solution to loaded carbon
Film diffusion — the [Au(CN)₂]⁻ complex crosses the solution boundary layer around each granule. Agitation controls this step.
Pore diffusion — the complex travels into internal pores. Granule size and pore structure control this step.
Adsorbimento superficiale — the complex binds to active sites. Surface chemistry and total area control this step.
2. Why hardness is a recovery parameter
A granule that breaks in a stirred tank shortens diffusion paths but creates gold-bearing fines that escape the adsorption circuit. In an abrasive ore, moving from a marginal product to one at ball-pan hardness ≥99% with AARL attrition ≤1.5% cuts fines generation directly. The AC50 verified data set is: 6×12 mesh, ball-pan ≥99%, AARL attrition ≤1.5%, platelet ≤5.0%, K ≥26 kg/t, R ≥50%, CTC ≥50%, butane ≥19.5%, ash ≤3.0%, moisture ≤5.0%, bulk density 0.48–0.55 g/mL. Iodine value is deliberately omitted — published figures conflict, so CTC and butane activity are the auditable measures.
Il Triangolo d'Oro: tre prodotti, un fornitore
AuCyan™ Cianuro di sodio NaCN (≥98.3%) · AuCarb™ Recupero dell'oro Carbone attivo da guscio di cocco (durezza ≥99%) · AuLeach™ Agente di lisciviazione dell'oro (GDA) – Non pericoloso
3. Worked calculation: the cost of fines
A 2,000 t/day CIL plant carries 12 tonnes of carbon with a 30-day cycle. At 1.5% attrition per cycle it loses about 180 kg per cycle, or 2.2 tonnes a year. At 3.0% it loses roughly 4.3 tonnes — a difference of 2.1 tonnes of carbon. If those fines carry even 200 g/t of gold, the annual gold difference is about 420 g. At any reasonable gold price, the hardness premium paid for the better carbon is smaller than the gold saved.
1.5% attrition: ≈ 2.2 t/year make-up carbon
3.0% attrition: ≈ 4.3 t/year make-up carbon
4. K and R are not the same number
K value is the adsorption rate constant — how fast gold loads. R value is equilibrium capacity — how much it holds. A high K with modest R suits short contact time. A high R suits a circuit that runs carbon to heavy loading before elution. Buying on either alone is a common and expensive mistake. Run bottle-roll loading on your own ore, set the K/R target from your contact time, then buy the lowest grade that reaches it.
5. Quattro livelli scolastici, quattro lavori
| Classe | Circuito | Definizione delle specifiche |
|---|---|---|
| BC1100 | Lisciviazione in cumulo / Carbonio in colonna | Elevata attività per soluzioni di grado inferiore |
| AC50 | Standard CIP/CIL | 6×12 mesh, K ≥26, R ≥50%, CTC ≥50% |
| AC55 | CIP/CIL a carico più elevato | K ≥28 kg/t, R ≥55% |
| AC60 | Premium CIP/CIL | K ≥30 kg/t, R ≥60%, 8×16 o 6×12 |
6. Rigenerazione e ciclo di vita
Loaded carbon is eluted and thermally regenerated before returning to the circuit. Every cycle imposes thermal and mechanical stress. Platelets and weak granules are preferentially lost in handling and regeneration. A carbon at ball-pan hardness ≥99% with platelet ≤5.0% typically sustains more cycles before make-up is required. Packing is Sacchi in PE laminato per carichi pesanti da 25 kg, with a batch COA, TDS and MSDS. Il MOQ è 1 container da 20' ≈ 15 tonnellate per FOB / CIF termini; United Chemical serve oltre 77 paesi.
5b. Screening and fines recovery
Attrition control does not end at the carbon specification. Screen condition determines whether a broken granule is removed cleanly or ground further and carried forward. A worn screen with oversized apertures passes loaded fines into the tailings stream; a blinded screen holds carbon in the tank too long and increases grinding. The practical routine is to log screen aperture, inspect panels on a fixed schedule and sample the carbon size distribution in the circuit monthly. If the proportion of sub-millimetre material is rising while make-up carbon is on budget, the problem is mechanical rather than metallurgical. Equally, gold-bearing fines caught on a screen are not lost; they should be routed to the elution circuit where the recovery economics justify it. This is why hardness and attrition numbers belong in an operating dashboard, not only in the purchase order.
7. FAQ
D1 — Cosa significa in pratica una durezza ≥99%?
Ball-pan hardness ≥99% means the granule resists mechanical breakdown to a defined standard, reducing fines.
Q2 — Which mesh size?
6×12 for agitated CIP/CIL, 8×16 where finer loading is needed, BC1100 for columns and heap.
D3 — Pubblicate i valori di iodio?
No — CTC and butane activity are the auditable pore measures because published iodine figures conflict.
D4 — Cosa viene spedito con ogni lotto?
Certificato di analisi (COA), scheda tecnica (TDS) e scheda di sicurezza (MSDS) del lotto in sacchi di PE laminato resistenti da 25 kg.
D5 — Qual è il quantitativo minimo d'ordine (MOQ)?
1 container da 20' ≈ 15 tonnellate, FOB o CIF.
Q6 — Can I test before buying?
Sì, campioni gratuiti di AuCarb™ e AuLeach™ per analisi di laboratorio indipendenti.
Measure your attrition loss
Tell us your circuit type, screen aperture and ore abrasiveness. We propose a grade, a K/R target and a test protocol.
Contattaci · AC50 · AC55 · AC60 · Panoramica del Triangolo d'Oro
WhatsApp +86 173 9270 5576 info@unitedchemicalcn.com
- Contenuto casuale
- Contenuti caldi
- Contenuto di recensioni hot
- Fabbrica cinese Acido solforico 98%
- Acido solforico 98% grado industriale
- Tubo antiurto in plastica (VOD≧1600m/s)
- Solfato ferroso grado industriale 90%
- I reagenti di flottazione hanno un impatto ambientale?
- 1Cianuro di sodio scontato (CAS: 143-33-9) per l'attività mineraria - Alta qualità e prezzi competitivi
- 2Cianuro di sodio 98.3% CAS 143-33-9 NaCN agente di rivestimento dell'oro essenziale per le industrie chimiche minerarie
- 3Nuove normative cinesi sulle esportazioni di cianuro di sodio e linee guida per gli acquirenti internazionali
- 4Cianuro di sodio (CAS: 143-33-9) Certificato per l'utente finale (versione cinese e inglese)
- 5Codice internazionale di gestione del cianuro (cianuro di sodio) - Standard di accettazione delle miniere d'oro
- 6Fabbrica cinese Acido solforico 98%
- 7Acido ossalico anidro 99.6% grado industriale
- 1Cianuro di sodio 98.3% CAS 143-33-9 NaCN agente di rivestimento dell'oro essenziale per le industrie chimiche minerarie
- 2Elevata purezza · Prestazioni stabili · Recupero più elevato: cianuro di sodio per la moderna lisciviazione dell'oro
- 3United ChemicalIl team di ricerca di dimostra autorevolezza attraverso approfondimenti basati sui dati
- 4Cianuro di sodio ad alte prestazioni AuCyan™ | Purezza del 98.3% per l'estrazione globale dell'oro
- 5Detonatore elettronico digitale (tempo di ritardo 0~ 16000ms)
- 6Detonatore a tubo d'urto ad alta resistenza e alta precisione
- 7industria Detonatore elettrico











Consultazione messaggi online
Aggiungi un commento: