UNITED CHEMICAL · PRODUKTTEKNIK · 27 NOVEMBER 2026
Ocuco-landskapet Kol you replace is not the carbon you lose
Fines carry gold out of the circuit, and they rarely appear on the purchase order.
Activated carbon is consumed two ways. It leaves as loaded carbon after elution, and it grinds into fines that report to tailings carrying adsorbed gold. The second loss is rarely budgeted. Ball-pan hardness and AARL attrition predict it; mesh size and platelet count predict how fast it happens in a given circuit. This guide uses AuCarb™ Gold Recovery kokosnötskal aktivt kol (≥99 % hårdhet) as the worked example.
1. Three steps from solution to loaded carbon
Film diffusion — the [Au(CN)₂]⁻ complex crosses the solution boundary layer around each granule. Agitation controls this step.
Pore diffusion — the complex travels into internal pores. Granule size and pore structure control this step.
Ytadsorption — the complex binds to active sites. Surface chemistry and total area control this step.
2. Why hardness is a recovery parameter
A granule that breaks in a stirred tank shortens diffusion paths but creates gold-bearing fines that escape the adsorption circuit. In an abrasive ore, moving from a marginal product to one at ball-pan hardness ≥99% with AARL attrition ≤1.5% cuts fines generation directly. The AC50 verified data set is: 6×12 mesh, ball-pan ≥99%, AARL attrition ≤1.5%, platelet ≤5.0%, K ≥26 kg/t, R ≥50%, CTC ≥50%, butane ≥19.5%, ash ≤3.0%, moisture ≤5.0%, bulk density 0.48–0.55 g/mL. Iodine value is deliberately omitted — published figures conflict, so CTC and butane activity are the auditable measures.
Gyllene triangeln – tre produkter, en leverantör
AuCyan™ Natriumcyanid NaCN (≥98.3 %) · AuCarb™ Gold Recovery kokosnötskal aktivt kol (≥99 % hårdhet) · AuLeach™ guldlakningsmedel (GDA) – Icke-farligt
3. Worked calculation: the cost of fines
A 2,000 t/day CIL plant carries 12 tonnes of carbon with a 30-day cycle. At 1.5% attrition per cycle it loses about 180 kg per cycle, or 2.2 tonnes a year. At 3.0% it loses roughly 4.3 tonnes — a difference of 2.1 tonnes of carbon. If those fines carry even 200 g/t of gold, the annual gold difference is about 420 g. At any reasonable gold price, the hardness premium paid for the better carbon is smaller than the gold saved.
1.5% attrition: ≈ 2.2 t/year make-up carbon
3.0% attrition: ≈ 4.3 t/year make-up carbon
4. K and R are not the same number
K value is the adsorption rate constant — how fast gold loads. R value is equilibrium capacity — how much it holds. A high K with modest R suits short contact time. A high R suits a circuit that runs carbon to heavy loading before elution. Buying on either alone is a common and expensive mistake. Run bottle-roll loading on your own ore, set the K/R target from your contact time, then buy the lowest grade that reaches it.
5. Fyra betyg, fyra jobb
| Grade | Krets | Definiera specifikationer |
|---|---|---|
| BC1100 | Höglakning / Kol i kolonnen | Hög aktivitet för lösningar av lägre kvalitet |
| AC50 | Standard CIP/CIL | 6×12 mesh, K ≥26, R ≥50%, CTC ≥50% |
| AC55 | CIP/CIL med högre belastning | K ≥28 kg/t, R ≥55% |
| AC60 | Premium CIP/CIL | K ≥30 kg/t, R ≥60 %, 8×16 eller 6×12 |
6. Regenerering och livscykel
Loaded carbon is eluted and thermally regenerated before returning to the circuit. Every cycle imposes thermal and mechanical stress. Platelets and weak granules are preferentially lost in handling and regeneration. A carbon at ball-pan hardness ≥99% with platelet ≤5.0% typically sustains more cycles before make-up is required. Packing is 25 kg kraftiga laminerade PE-påsar, with a batch COA, TDS och MSDSMOQ är 1×20' FCL ≈ 15 MT under FOB / CIF villkor; United Chemical betjänar mer än 77 länder.
5b. Screening and fines recovery
Attrition control does not end at the carbon specification. Screen condition determines whether a broken granule is removed cleanly or ground further and carried forward. A worn screen with oversized apertures passes loaded fines into the tailings stream; a blinded screen holds carbon in the tank too long and increases grinding. The practical routine is to log screen aperture, inspect panels on a fixed schedule and sample the carbon size distribution in the circuit monthly. If the proportion of sub-millimetre material is rising while make-up carbon is on budget, the problem is mechanical rather than metallurgical. Equally, gold-bearing fines caught on a screen are not lost; they should be routed to the elution circuit where the recovery economics justify it. This is why hardness and attrition numbers belong in an operating dashboard, not only in the purchase order.
7. FAQ
F1 — Vad betyder ≥99 % hårdhet i praktiken?
Ball-pan hardness ≥99% means the granule resists mechanical breakdown to a defined standard, reducing fines.
Q2 — Which mesh size?
6×12 for agitated CIP/CIL, 8×16 where finer loading is needed, BC1100 for columns and heap.
F3 — Publicerar ni jodvärdet?
No — CTC and butane activity are the auditable pore measures because published iodine figures conflict.
Q4 — Vad medföljer varje batch?
Batch-COA, TDS och MSDS i 25 kg kraftiga laminerade PE-påsar.
Q5 — Vad är MOQ?
1×20' FCL ≈ 15 ton, FOB eller CIF.
Q6 — Can I test before buying?
Ja — kostnadsfria prover av AuCarb™ och AuLeach™ för oberoende laboratorietester.
Measure your attrition loss
Tell us your circuit type, screen aperture and ore abrasiveness. We propose a grade, a K/R target and a test protocol.
Kontakta oss · AC50 · AC55 · AC60 · Översikt över Gyllene Triangeln
WhatsApp +86 173 9270 5576 info@unitedchemicalcn.com
- Slumpmässigt innehåll
- Hett innehåll
- Hett recensionsinnehåll
- Kina fabrik svavelsyra 98%
- Svavelsyra 98% industriell kvalitet
- Stötrör i plast (VOD≧1600m/s)
- Järnsulfat industriell kvalitet 90 %
- Har flotationsreagenser miljöpåverkan?
- 1Rabatterad natriumcyanid (CAS: 143-33-9) för gruvdrift - hög kvalitet och konkurrenskraftiga priser
- 2Natriumcyanid 98.3% CAS 143-33-9 NaCN guldförbandsmedel viktigt för gruvkemisk industri
- 3Kinas nya regler för export av natriumcyanid och vägledning för internationella köpare
- 4Sodium Cyanide (CAS: 143-33-9) Slutanvändarcertifikat (kinesisk och engelsk version)
- 5Internationell cyanid(Natriumcyanid) Management Code - Gold Mine Acceptance Standards
- 6Kina fabrik svavelsyra 98%
- 7Vattenfri oxalsyra 99.6% industriell kvalitet
- 1Natriumcyanid 98.3% CAS 143-33-9 NaCN guldförbandsmedel viktigt för gruvkemisk industri
- 2Hög renhet · Stabil prestanda · Högre återvinning — natriumcyanid för modern guldurlakning
- 3United Chemicals forskarteam visar auktoritet genom datadrivna insikter
- 4AuCyan™ högpresterande natriumcyanid | 98.3 % renhet för global guldbrytning
- 5Digital elektronisk sprängkapsel (Fördröjningstid 0~16000ms)
- 6Höghållfast, hög precision Shock Tube Detonator
- 7industri elektrisk sprängkapsel











Online meddelandekonsultation
Lägg till kommentar: